6082 aluminum plate in the oxidation, need to understand some common sense of oxidation, the 6082 aluminum plate manufacturers to introduce the common sense of oxidation.
First of all, before oxidation, it is necessary to check the advantages and disadvantages of the material and its composition, which will affect the effect of oxidation. If there are bubbles, scratches and other defects on the surface of 6082 aluminum plate, the defects will be exposed after anodic oxidation.
Different ingredients, the effect of oxidation is not the same:
Aluminum alloys containing 1 ~ 2% manganese are brownish blue after oxidation, and the color changes from brownish blue to dark brown with the increase of manganese content.
Aluminum alloy containing 0.6 ~ 1.5% silicon is gray after oxidation, and white gray when containing 3 ~ 6% silicon.
Those containing zinc have an opaque color, those containing chromium have an uneven hue of golden to gray, and those containing nickel have a pale yellow.
Generally speaking, aluminum containing magnesium and titanium content of more than 5% gold, after oxidation can get colorless transparent and bright, smooth appearance.
6082 aluminum plate oxidation of common sense on this, want to know the price of 6082 aluminum plate can consult us.